Scanning Electron Microscopy (SEM) images of the ZnO nanorod sample shown in Figures 3 (courtesy of Bell Labs, Lucent Technologies). Image magnification is 15,000x for figure (a) and 30,000x for figure (b), respectively. A 45 degrees sample tilt was employed.